Table of content
What Is Alloy Steel?
Alloy steel has chromium, boron, molybdenum, silicon, vanadium, aluminum, nickel content. These elements increase toughness and corrosion resistance properties, there are two types one is high alloy steel has more % of alloying elements and another is low alloy steel has less % of alloying elements. Alloy steel material is mainly used in aerospace, construction and mining industry
What Is Carbon Steel?
Carbon steel material has iron and carbon content. There are three types of CS they are low (0.25% carbon content), medium ( 0.25% to 0.6% ) and high (0.6-1.25%). CS is mainly used for shipbuilding, construction and pressure Vessels applications
| Pipe | |||
|---|---|---|---|
| ASTM A53 garde A | ASTM A106 garde A | ASTM A500 grade B | ASTM A134 |
| ASTM A53 garde B | ASTM A500 grade C | ASTM A106 garde C | ASTM A333 garde 6 |
| ASTM A252 Gr. 1 | ASTM A252 Gr. 2 | ASTM A252 Gr. 3 | ASTM A500 grade A |
| ASTM A333 garde 1 | ASTM A106 garde B | ||
| Tube | |||
| ASTM A513 Grade 1 | ASTM A500 Grade A | ASTM A513 Grade 2 | ASTM A500 Grade B |
| ASTM A500 Grade C | ASTM A179 | ASTM A214 | |
| Sheet and Plate | |||
| ASTM A36 | ASTM A1011 | ASTM A283 Grade C | ASTM A516 Grade 70 |
| ASTM A572 Grade 50 | ASTM A516 Grade 60 | ASTM A516 Grade 65 | |
| Flanges and Fittings | |||
| ASTM A234 WPB | ASTM A234 WPC | ASTM A350 LF2 | ASTM A694 F52 |
| ASTM A105 | ASTM A181 | ASTM A234 WP1 | ASTM A234 WP9 |
| Chrome Molybdenum Steel | |||
| Supply condition : |
| Application : |
|
| ASTM A387 | Grade 12 | Grade 22 | Grade 11 |
| Grade 5 | Grade 9 | Grade 91 | |
| EN 10028 -2 | DIN 17175 | SAE 4130 | ASTM A204 |
| ASTM A302 | SAE 8620 | SAE 4140 | EN 24 |
| EN 19 | EN 36 | EN 10028 -2 | DIN 17175 |
| Wear Resistant Steel | |||
| Supply condition : |
| Application : |
|
| 200HB | 300HB | 400HB | 500HB |
| High Tensile Steel | |||
| Supply condition : |
| Application : |
|
| EN 10025-2 – | S355 | S420 | S460 |
| IS 2062 – | E350 | E450 | E410 |
| Quenched and Tempered Steel | |||
| Supply condition : |
| Application : |
|
| EN 10025-6- | S500 | S620 | S550 |
| Tool Steel | |||
| Supply condition : |
| Application : |
|
| H11 | A2 | O1 | D3 |
| D2 | HCHCR | S-13 | |
| Other Alloy Steels | |||
| Supply condition : |
| Application : |
|
| 16/20MnCr5 | EN1A | EN52 | EN31 |
| EN41 | 42CrMo4 | ||
| Pipe | |||
|---|---|---|---|
| ASTM A53 garde A | ASTM A106 garde A | ASTM A333 garde 1 | ASTM A134 |
| ASTM A500 grade B | ASTM A106 garde B | ASTM A500 grade C | ASTM A333 garde 6 |
| ASTM A252 Gr. 1 | ASTM A252 Gr. 2 | ASTM A252 Gr. 3 | ASTM A500 grade A |
| ASTM A53 garde B | ASTM A106 garde C | ||
| Tube | |||
| ASTM A513 Grade 1 | ASTM A500 Grade A | ASTM A513 Grade 2 | ASTM A500 Grade B |
| ASTM A179 | ASTM A214 | ASTM A500 Grade C | |
| Sheet and Plate | |||
| ASTM A36 | ASTM A1011 | ASTM A283 Grade C | ASTM A516 Grade 70 |
| ASTM A572 Grade 50 | ASTM A516 Grade 60 | ASTM A516 Grade 65 | |
| Flanges and Fittings | |||
| ASTM A234 WPB | ASTM A234 WPC | ASTM A350 LF2 | ASTM A694 F52 |
| ASTM A105 | ASTM A181 | ASTM A234 WP1 | ASTM A234 WP9 |
| ASTM Standard | ASTM A335 | ASTM A519 | ASTM A829 | ASTM A830 |
|---|---|---|---|---|
| Brinell Hardness | 197 – 290 | 190 – 290 | 207 – 540 | 170 – 210 |
| Rockwell Hardness | 25 – 37 | 22 – 37 | 28 – 60 | 25 – 30 |
| ASTM A234 | ASTM A350 LF2 | ASTM A105 | ASTM A694 | |
| Brinell Hardness | 200 – 230 | 180 – 210 | 170 – 210 | 250 – 300 |
| Rockwell Hardness | 28 – 30 | 22 – 26 | 25 – 30 | 30 – 35 |
| ASTM Standard | A106 Grade B | A53 Grade B | A500 Grade B | A513 Type 5 |
|---|---|---|---|---|
| Brinell Hardness | 155-185 | 150-190 | 150-200 | 170-210 |
| Rockwell Hardness | 20-24 | 23-28 | 23-30 | 25-30 |
| A500 Grade C | A36 | A1011 | A36 | |
| Brinell Hardness | 150-200 | 119-160 | 145-185 | 119-160 |
| Rockwell Hardness | 23-30 | 20-25 | 20-30 | 20-25 |
| A572 Grade 50 | ASTM A234 WPB | ASTM A350 LF2 | A105 | |
| Brinell Hardness | 170-210 | 200-230 | 180-210 | 170-210 |
| Rockwell Hardness | 25-30 | 28-30 | 22-26 | 25-30 |
Alloy Steel Material Properties And Characteristics


| Parameters | Carbon Steel | Alloy Steel |
|---|---|---|
| Corrosion resistance | Poor | Poor |
| Hardness | High | Low |
| Malleability | High | Low |
| Toughness | High | Low |
| Ductility | Low | High |
| Cost | Lower Than Alloy Steel | Higher Than Carbon Steel |
| Tensile strength | Up to 450 MPa | up to 960 MPa |
| Magnetism | depend on carbon content | magnetic |
| Melting point | 1425 to 1530°C | 1400 to 1500°C |
| Heat resistance | Fair | High |
| Heat treatable | Yes | Yes |
| Ductility | Fair | Good |
| Type |
|
|
| Properties | Less versatile | More versatile |
| Composition | iron and less than 2% carbon content |
|
| Stronger | Less | More |
Carbon Steel Chemical Composition
| Gr. | A106 gr B | A53 gr B | API 5L X52 | API 5L X42 | A36 | A572 gr 50 | A516 gr 70 | A182 F304 | A105 | A403 WP304 | A500 gr B | A234 WPB | A1011 | 1080 | A1008 | A513 | 1045 | 1010 | 1060 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Carbon %(C) max | .30 to .35 | .25 to .30 | .22 | .26 | .26 to .29 | .23 to .28 | .26 to .29 | .08 | .25 to .30 | .08 | .26 to .29 | .25 to .30 | .05 to .15 | .75 to .85 | .09 to .15 | .18 | .43 to .50 | .08 to .13 | .55 to .65 |
| Manganese % (Mn) max | .10 to .40 | .40 to .80 | 1.20 | .40 to .80 | .60 to .90 | 1.35 to 1.65 | .60 to .90 | 2.00 | .30 to .60 | 2.00 | .40 to .80 | .40 to .80 | .40 | .60 to .90 | .40 | .30 to .60 | .60 to .90 | .30 to .60 | .60 to .90 |
| Silicon % (Si) max | .10 | .10 | .10 | .10 | .20 | .15 | .10 | .30 | .10 | .30 | .20 | .10 | .15 | .10 | .15 | .20 | .10 | .15 | .10 |
| Phosphorus % (P) max | .025 | .025 | .030 | .030 | .04 | .04 | .025 | .045 | .04 | .045 | .03 | .04 | .04 | .04 | .04 | .04 | .04 | .04 | .04 |
| Sulfur %(S) max | .025 | .015 | .030 | .030 | .05 | .05 | .01 | .030 | .05 | .030 | .03 | .05 | .05 | .05 | .05 | .05 | .05 | .05 | .05 |
| Grade | A335 P22 | A335 P11 | A1010 | A387 Gr 11 | A519 4140 | 4340 | A519 4130 | A182 F11 | A387 Gr 22 | A1008 | 8620 | A234 WP5 | A182 F5 | 4140 | A234 WP1 | A519 4140 | A519 4340 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Mn % max | .30 to .60 | .30 to .60 | .30 | .30 to .60 | .75 to 1.00 | .60 to .90 | .40 to .80 | .30 to .60 | .30 to .60 | .40 | .60 to .90 | .20 to .40 | .20 to .40 | .75 to 1.00 | .40 to .80 | .75 to 1.00 | .60 to .90 |
| C % max | .05 to .15 | .05 to .15 | .06 to .12 | .05 to .15 | .38 to .43 | .38 to .43 | .28 to .33 | .05 | .05 to .15 | .09 to .15 | .18 to .23 | .05 | .05 | .38 to .43 | .15 | .38 to .43 | .38 to .43 |
| Cr % max | 1 to 1.50 | 1 to 1.50 | .50 | 1 to 1.50 | .80 to 1.10 | .70 to .90 | .40 to .60 | 1 to 1.50 | 1 to 1.50 | .50 | .70 to .90 | 4 to 5.00 | 4 to 5.00 | .80 to 1.10 | 1 to 1.50 | .80 to 1.10 | .70 to .90 |
| S % max | .025 | .025 | .05 | .025 | .040 | .040 | .040 | .025 | .025 | .05 | .040 | .030 | .030 | .040 | .05 | .040 | .040 |
| P % max | .025 | .025 | .04 | .025 | .040 | .040 | .040 | .025 | .025 | .04 | .040 | .045 | .045 | .040 | .04 | .040 | .040 |
| Si % max | .10 | .10 | .20 | .10 | .15 | .15 | .20 | .10 | .10 | .15 | .15 | .30 | .30 | .15 | .10 | .15 | .15 |
| Ni % max | .40 | .40 | .50 | .40 | .20 | 1.50 to 2.00 | .40 | .40 | .40 | .50 | .50 to .70 | .50 | .50 | .20 | .40 | .20 | 1.50 to 2.00 |
| Mo % max | .87 to 1.05 | .40 to .60 | .10 | .40 to .60 | .15 to .25 | .20 to .30 | .10 to .20 | .40 to .60 | .87 to 1.05 | .10 | .15 to .25 | .15 | .15 | .15 to .25 | .40 | .15 to .25 | .20 to .30 |
Welding process of Carbon and Alloy Steel
| Welding process | CS | AS |
|---|---|---|
| Shielded Metal Arc Welding | E6010 | Require specific fillers |
| E7018 | ||
| Gas Tungsten Arc Welding | ER70S-2 | |
| Gas Metal Arc Welding | ER70S-6 | |
| Submerged Arc Welding | ||
| Flux-Cored Arc Welding | E71T-1 |
Carbon and alloy steel density

Which Steel is Better in Water Desolation Plants
As compare to CS, alloy steel is better option to choose in water desolation plants because of its material properties such as :
Quenched and Tempered Properties of Carbon and Alloy Steel
| Q & T Carbon Steel | Q & T Alloy Steel |
|---|---|
| Improved stability after Q & T | Enhanced stability due to HT |
| Increased strength after quenching | Increased strength due to quenching |
| Increased hardness after quenching | Higher hardness due to quenching |
| Improved toughness due to HT | Improved toughness after tempering |
Alloy and Carbon Steel Mechanical Properties

Medium Carbon Steel Heat Treatment
Low Carbon Steel Temperature Range
| Type | Carbon content | Normalizing (°C) | Annealing (°C) | Tempering (°C) | Quenching (°C) | Stress Relieving (°C) |
|---|---|---|---|---|---|---|
| Low CS | Less than 0.3% | 800 to 900 | 600 to 700 | 150 to 600 | 800 to 900 | 300 to 500 |
| Medium CS | 0.3 to 0.6% | 850 to 950 | 700 to 800 | 150 to 650 | 800 to 900 | 400 to 600 |
| High CS | More than 0.6% | 850 to 950 | 700 to 800 | 200 to 700 | 800 to 1,000 | 400 to 600 |
Alloy steel vs non alloy steel

Which one is stronger carbon steel or alloy steel?
Alloy steel is more stronger than carbon steel. Tensile strength of AS is higher than CS, Alloy steel strength range between 758 to 1882 MPa
Which is better carbon steel or alloy steel?
Its totaly depend on your project requirements. Choose alloy steel if you require better corrosion resistance and also suitable for high stress environments. Choose carbon steel if you looking for a low cost and suitable for construction and structural applications.
What factors should be considered when choosing between CS and AS?
What are the applications where the carbon steel preferred over alloy steel?